Drawing with Frit, Drawings, Expirimentation, Frit, Fusing, Glass

Drawing with Frit.

The first non-test firing in the new kiln. Kiln works! Woot!

Nothing complicated. Black powder on Bullseye Tekta.
After Firing! not much different. except now it won’t blow away!
This programmer works on Rate/Hold, so I’m using that now… and I still like Celsius better.
Firing Program:
Currently Program 1 on Kiln
1. 333C/H to 745C hold 00:10
2. AFAP to 482C hold 1:00
3. 55C/H to 371C hold 00:00
4. AFAP to 21C hold 00:00

Leave a Reply